Yes if performed in accordance with the requirements of A-999
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
"Eric.C" ---07/05/2015 08:43:18---Hi All, Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6.
From: "Eric.C" <ericheng87@gmail.com>
To: materials-welding@googlegroups.com
Date: 07/05/2015 08:43
Subject: [MW:23220] Eddy Current vs Hydrotest for LTCS pipes (A333 Gr.6)
Sent by: materials-welding@googlegroups.com
Hi All,
Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6.
Is ET acceptable in lieu of hydrotest? if yes, is there any limitation criteria?
Thanks.
Regards,
Eric.C
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/725e2e6d-7969-4d55-ab84-a02452545612%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.