Re: [MW:23223] Eddy Current vs Hydrotest for LTCS pipes (A333 Gr.6)

it is acceptable .

On Thu, May 7, 2015 at 5:24 AM, Eric.C <ericheng87@gmail.com> wrote:
Hi All,

Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6.
Is ET acceptable in lieu of hydrotest? if yes, is there any limitation criteria?
Thanks.

Regards,
Eric.C

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/725e2e6d-7969-4d55-ab84-a02452545612%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAErPVf1QzFWM-b1ocvBbXVzsqa3WyQTUL0kNF3u1G_kWCrhGbQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...