Re: [MW:23221] Re: Equivalent ASTM material for EN S275JR

Dear,

you cannot get exact equivalent.

But nearby grade is ASTM A36   

ELAVARASAN ARUMUGAM
Mechanical Engineer 
 

On Wed, May 6, 2015 at 9:45 AM, R R Menon <ranjith.rajeevan@gmail.com> wrote:
Hiii

its equivalent to ASTM A529

On Saturday, 23 July 2011 15:16:35 UTC+3, PRAMODH NAIR wrote:
Experts,
 
Could you please give me the equivalent ASTM material for EN S275JR with reference code document.
 
Regards
Pramodh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/394a3b77-8a49-4504-8a9f-4c150b4ba3d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKBH9tOZvYuRxtLGNZUS5YT7jAzyxraKxs1FRFrpvPoO3%2BF5tA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...