Dear Pramodh;
The equivalent is A 520 .
S 275 Jr is europeen normalisation , S means Structure , 275 is the yield strength JR means 27 j at room temperature for impact test.
REgards
SALHI Raouf
QA/QC Engineer
Tel: Morocco +212628979891
Tunisia +21621458258
Le Mercredi 6 mai 2015 10h59, Harikrishnan N S <hari.qaqc@gmail.com> a écrit :
Hi Pramodh
You may refer ASTM document DS67 for comparing different Steel standards. But you may not find the exact equivalent.
Thanks and Regards
Harikrishnan
On Saturday, July 23, 2011 at 8:16:35 PM UTC+8, PRAMODH NAIR wrote:
Experts,Could you please give me the equivalent ASTM material for EN S275JR with reference code document.RegardsPramodh
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b0cb2650-1d8e-4bcc-8844-6541b3740534%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment