Wednesday, May 6, 2015

Re: [MW:23213] Max.Base metal thickness qualified

The qualified thickness are as follows:

Thinner member: from 5 mm to 40 mm
Thicker member: no limitation

Please refer to QW-202.4 in Section IX of ASME BPVC

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Hrushikesh Sangamnerkar ---05/05/2015 15:21:53---Dear experts, I have a P8 # P43 PQR.

From: Hrushikesh Sangamnerkar <hrushi612@gmail.com>
To: materials-welding@googlegroups.com
Date: 05/05/2015 15:21
Subject: [MW:23208] Max.Base metal thickness qualified
Sent by: materials-welding@googlegroups.com





Dear experts,
I have a P8 # P43 PQR.
Joint design = Single V
Base metal thickness for P8 = 40mm and for P43 = 20mm.
What should be the Max.Base metal thickness range qualified for such joint?

Regards,
Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAMpWL2oHcKgDYmxWs9gVLaM8WLSSCewN4XcECCjVs6i8fkr7jw%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...