Wednesday, May 6, 2015

[MW:23212] Re: Equivalent ASTM material for EN S275JR

Hiii

its equivalent to ASTM A529

On Saturday, 23 July 2011 15:16:35 UTC+3, PRAMODH NAIR wrote:
Experts,
 
Could you please give me the equivalent ASTM material for EN S275JR with reference code document.
 
Regards
Pramodh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/394a3b77-8a49-4504-8a9f-4c150b4ba3d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...