PTC requirements are mentioned in UG 89 (i) of ASME Sec VIII-Div I & Para 3.11.8.4 of ASME Sec VIII-II.

Regds/Jignesh

On Tuesday, 5 May 2015 16:30:51 UTC+5:30, kashif syed wrote:
Dear All,

Good day


We are doing welding on a spherical vessel. The client is asking for the production weld sample for the first 3m of welding for all the joints along with the RT.

My questions are:
1. Where is the detail reference for requirement of production test coupon in ASME Sec IX?

2. Can we replace RT with PAUT ? Is there any specific technical requirement that only RT needs to be done not PAUT on PTC. as in actual job we will be doing PAUT not RT.

Waiting for your genuine reply. 

--
Thanks & Regards,


Syed Kashif Farhan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8384700b-405d-49f5-89dc-77fa5c526a45%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...