244 Hv should be ok,


Date: Tue, 5 May 2015 20:49:24 +0800
Subject: Re: [MW:23209] RE: 23206] Failed SSC test
From: amirzakee@gmail.com
To: materials-welding@googlegroups.com; materials-welding@googlegroups.com

Hi Alan
Based on the same WPQT but conducted on different test coupon the highest hardness value is 244 on the HAZ side.
Do you reckon hardness is the issue?

Thanks.
Amir Zakee

Sent from my BlueBerry 10 semakphone.
From: Alan Denney
Sent: Selasa, 5 Mei 2015 20:23
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: [MW:23207] RE: 23206] Failed SSC test

Boxbe This message is eligible for Automatic Cleanup! (alan@denney1.freeserve.co.uk) Add cleanup rule | More info


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20150505124924.5226578.81037.23477%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...