Dear Experts,
We are observing crqcks during. Tack welding for setup between material casting. BS3100 Gr A4
And D 40 S.
Electrode using is. E8018-C1 and preheat is 150 degree and also. Done postheating because of repeatedly observing cracks again and again
Pls give your suggestions to avoid cracks.
Best Regards,
Mohit Aggarwal..
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment