If the tank ur building don't require PWHT or Thermal Stress Relieve as its been named in API 650 then u don't need to requalify ur wps but also remember, PWHT is required on the the clean out flush out door irrespective of the metal group and the assembly to be done separately. Group I,II,III metals do not need PWHT but the Clean-out-flush out door need to be thermal stress relieve so it can be done separately. Yet the WPS don't need requalification I suppose. 


On Thu, Apr 17, 2014 at 6:04 PM, Bala Murugan <balamuruganqaqc@gmail.com> wrote:
Dear Marat,
If your job not required any PWHT then you no need to qualify your wps
with PWHT.As i worked with API 650 Iam very much confident about it.
 And API 650 deals only with carbon plated oil tanks not plastics.

Thanks,
BALAMURUGAN M,
L&T,
INDIA,
PH +91 8763569606

On 4/17/14, george.dilintas@gr.bureauveritas.com
<george.dilintas@gr.bureauveritas.com> wrote:
>
> If Thermal Stress Relief (PWHT) is not required by API 650, then you have
> not to perform a PWHT on your PQR specimen
>
> best regards
>
> Dr. Georgios Dilintas
>
> Authorized Nuclear Inspector
> Authorized Inspector Supervisor
> API 510 Inspector
>
> I&F REGIONAL TECHNICAL MANAGER
> BUREAU VERITAS HELLAS
>
> Tel: +30 210 40 63 113/4
> Fax: +30 210 40 63 118
> Cell: +30 69 44 64 62 04
> (See attached file: Dilintas_George.vcf)
>
>
>
> From: Marat Nurbekov <marat.nurbekov@gmail.com>
> To:   materials-welding@googlegroups.com
> Date: 16/04/2014 15:56
> Subject:      [MW:20597] WPS as per API 650
> Sent by:      materials-welding@googlegroups.com
>
>
>
> HI Dear Members,
> Could you help me? I work in project for Crude Oil Tank. The tank shall be
> constructed as per API650 and now I have some following doubts:
> 1) As you know WPS for API 650 has to be qualified as per ASME IX CODE and
> as per this code PWHT is essential variable but what about Thermal Stress
> Relief which is required as per API 650?
> Shall I qualify WPS with Thermal Stress Relief or Thermal Stress Relief
> shall be performed when it is required as per API 650
> 2) For Crude Oil Tank shall be constructed Fire water pipe system and
> Drainage system. Company is going to use a plastic pipe material but there
> are not any notes regarding plastic materials in ASME IX and API 650.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding
> +unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>
> This message contains confidential information. To know more, please click
> on the following link: http://disclaimer.bureauveritas.com
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...