[MW:16538] API 6A- PQR qualification for weld overlay - Automatic PAW process

Dear Sir,
Pls , help out in following query:-
As per API-6A Stds requirements :-
1) We require to Clad/overlay 4mm Inconel-625 on inside (Bore)WCB A216 grA Body (uncomplete Valve).
2) Pls , guide on "selection of PQR qualification " i.e Pipe or Plate.(A216 GrA)
3) Actual Production Welding will be on Automatic PAW machine & Position is 1G (Downhand) -ROTATION, But Valve will on Rotation position (1G-R) during welding.(Automatic)
4) Pls , guide & tell me regarding selection of PQR Form i.e. Pipe or Plate (Also the reason ) 
 
My QC head instructed me to do Traling mail qualification as per both Section -IX & As per EN-15614-7. in single test coupon (Query is follwing point as EN Std)
In EN-15614-7 , Overlay cladding /Hardfacing is defined as
a) Axial Overlay welding-inside/outsidE
b) Circumferential overlay Welding-Inside /outside
I anticipating , that EN Std means to say , If Production weld is Circumferetial (Rotation/or Not rotated) .
that means I Mean to say :- It will make a Big difference in depositing /to be qualified for either Axial or Circumferential.(rotated or no rotated)
Becaause our actual production weld requirment is Circumferential -Rotated.
 
Also, in our Plant PAW-Automatic machine has/is a Circumferential Rotary Positioners .So weld will be generated in Circumferentially around the Plate
PAW machine is design  for Inner Claading /inside bore of Valve (Valve Shape is in Circular/Circumferenial)
I.e We have to place plate  in such a way that Weld should place like Transverse 1G position/type of weld ..
 
But During PQR Side bend results in my presence :- Inconel Overlayed on WCB plate got Cracked in overlap of one layer another (30% Overlap).
I.e We cant do overlap automatically in While Boom (Torch Shifting) is not possible in Transverse type of Weld.
I.e During overlapping of  Each layer :- we mover torch fully automatically to lenght up to  150 mm.After reaching 150 mm , we would have to stop torch & machine & take reverse the Boom(Torch)or Welding poistioners to starting points.
 
I am anticipating thats why I am not getting desired results in Side bends.
 
Pls , guide in this case
Thats Why Idea glow in my mind to shift PQR form from Plate to Pipe.
So , there is No need to Stop torch after reaching 150 mm .Torch will shift automaticaaly as per CNC programme to 150 mm ..(as machine is designed for circumferential type of weld for Claddingof Valves & Pipes)
 
# If above Selection of PQR form i.e Pipe is OK.
Pls , guide on "Selection of Pipe OD with SCH for Qualifying Valve from 4 Inch to 40 Inch & Weld thickness deposited Qualification of min 4 to 5 mm , Our customer requirment of weld thickness depositions is 3.2 mm after machining."
 
 
Thankyou in advance
 
With Regards,
Ashish P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...