Thursday, August 9, 2012

[MW:15049] Acceptance criteria for Tungsten Inclusion in RT

Dear Friends
 
After reviewing a RT film of a Circ.seam joint (16mm thk), which has been welded with TIG + SMAW, i have observed a tungsten inclusion @2-3mm in dia.
The construction code of the vessel is ASME Sec VIII Div.1
 
No doubt this tungsten inclusion is a defect, but i would like to know whether there is any acceptance criteria related to diameter for the same in ASME Sec VIII Div.1. Please give Code reference.
 
Regards
 
Prem Nautiyal
Cell: 9769316004
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...