Re: [MW:13114] Minimum acceptance criteria for weld reinforcement for pipe and plate

dear friend
u must check the reinforcement as per wps. you are right, in general it is 1.6 to 3 mm,but cap reinforcement can be more(i.e 4mmm) in thicker pipes or plates.
regard
Mehdi Emami


From: md jamil ahmad <jamilmech2009@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, November 30, 2011 1:21 PM
Subject: [MW:13113] Minimum acceptance criteria for weld reinforcement for pipe and plate

Dear All,
          Any body explain me,1) what is the minimum acceptance criteria for out side weld reinforcement for power piping or process piping
          I think,in general 1.6 to 3mm,is it correct or not.
         2) In inside welding of pipe what is the minimum and maximum reinforcement criteria,please tell me as per ASME Code.


REGARD
JAMIL AHMAD
KSA
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...