Dear Soumya,
 
You can use PMI machine.Use Spark type machine with ultra pure Argon gas instead of X-ray fluorascense type.Purity of Argon gas is important as it will affect the result.
 
Regards,
 
Limesh

On Thu, Sep 16, 2010 at 3:28 PM, soumya podder <soumya.podder@gmail.com> wrote:
Dear Sir ,
 
Pls explain how we check the material of SS like SS 316 or SS 304 .

--
Thanks & Regards

Soumya Podder
9099982514

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...