Dear Soumya Podder,
 
The easy way of checking and identifying the difference between SS 316 and SS 304 is by MOLY TESTING, when you drop a moly solution on the material and charge with a battery the drop colour changes to pink and stands still if it is SS316 ELSE the colour changes to black after few minutes if it is SS 304.
 
Regards,
 
J.N.,MURTHY

On Thu, Sep 16, 2010 at 3:28 PM, soumya podder <soumya.podder@gmail.com> wrote:
Dear Sir ,
 
Pls explain how we check the material of SS like SS 316 or SS 304 .

--
Thanks & Regards

Soumya Podder
9099982514

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...