Thursday, September 16, 2010

Re: [MW:7050] Method for checking SS Material

Dear Soumya,
 
First of all if you have Test certificate in hand you just refer the chemical properties of 316 & 304 and corellate with TC. if it is satisfactory and then go for PMI or Spectro what ever is available for material confirmation. if both or not avialable then go for sample testing. and send the sample to lab for chemical analyisis.

--- On Thu, 16/9/10, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: Re: [MW:7046] Method for checking SS Material
To: materials-welding@googlegroups.com
Date: Thursday, 16 September, 2010, 10:02 PM

Dear Soumya,
 
You can use PMI machine.Use Spark type machine with ultra pure Argon gas instead of X-ray fluorascense type.Purity of Argon gas is important as it will affect the result.
 
Regards,
 
Limesh

On Thu, Sep 16, 2010 at 3:28 PM, soumya podder <soumya.podder@gmail.com> wrote:
Dear Sir ,
 
Pls explain how we check the material of SS like SS 316 or SS 304 .

--
Thanks & Regards

Soumya Podder
9099982514
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...