Re: [MW:5194] Welding of an attachment directly on the weld overlay

You can do this by making sure that the weld to be welded on is clean and smooth to prevent any inclusions, you can use  your orginal WPS.
 


 
On Tue, May 18, 2010 at 8:36 AM, fer <fernando.alvarez.fdez@gmail.com> wrote:
ASME VIII div 2 allows you to weld an attachment directly on the weld
overlay of a pressure vessel.

How should be qualified the WPS to carry out this welding?

The coupon of the PQR should be done with a buttering between the
material of the shell and the material of the attachment?

Could be asigned a P number to the weld overlay material and weld the
coupon between the P number of the overlay material and the P number
of the attachment?

Any idea would be helpful

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...