Tuesday, May 18, 2010

[MW:5193] Welding of an attachment directly on the weld overlay

ASME VIII div 2 allows you to weld an attachment directly on the weld
overlay of a pressure vessel.

How should be qualified the WPS to carry out this welding?

The coupon of the PQR should be done with a buttering between the
material of the shell and the material of the attachment?

Could be asigned a P number to the weld overlay material and weld the
coupon between the P number of the overlay material and the P number
of the attachment?

Any idea would be helpful

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...