Hi,
The repair rate calculation can use the rejected RT film agains total RT film..It is more make sense comparing base on joint which is too strenght and by lenght wise which is too easy..
Till now no such international standard regulate of repair rate calculation, it will be specified base on Owner/ Client spec..
CMIIW..
Regards..
Powered by Telkomsel BlackBerry®
From: james gerald <gerry_tup@yahoo.com>
Sender: materials-welding@googlegroups.com
Date: Sat, 15 May 2010 19:37:52 -0700 (PDT)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:5184] RE: 5170] welding Repair percentage
Soliman, When you try to take in Joint wise calculation the Repair rate percentage will be very high above the requirement of 3% or 5% normally specified. Stick to Length wise calculation
J.GERALD JAYAKUMAR 00919344954677
--- On Sat, 5/15/10, Soliman, Mohamed (kuwait) <Mohamed.Soliman@WorleyParsons.com> wrote: From: Soliman, Mohamed (kuwait) <Mohamed.Soliman@WorleyParsons.com> Subject: [MW:5179] RE: 5170] welding Repair percentage To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com> Date: Saturday, May 15, 2010, 4:31 AM
My contractor is proposing the calculation by the linear length wise .I disagreed with them and I am insisting the joint wise to have more control .I need any international standards that can support my situation as the owner specification does not specify the requirements. Please remember this only for plant piping welding and we have different sizes from 84 inches till 1 inch, Maximum of the lines is sour services. Regards Soliman From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of Prabhu Kumar L Sent: Friday, May 14, 2010 1:25 PM To: materials-welding@googlegroups.com Subject: [MW:5171] RE: 5170] welding Repair percentage Dear Soliman, % weld repair based on linear length will be calculated as follows: Total length (mm) of the weld radiographed against total length (mm) of repairs which will give you the % of repair in length wise. In this you need to calculate the length of each repair based on RT film. The % of repair will be very low in length wise compared to joint wise. As you indicted, joint wise is more practical compared to length wise. Regards, From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of mohamed soliman Sent: Friday, May 14, 2010 3:35 PM To: materials-welding@googlegroups.com Subject: [MW:5170] welding Repair percentage We are building new booster station ,our contractor wanted to calculate the repair percentage of the welding based on the linear lenght .Alwyas this should be calculated by the joint wise .Can any one refere any international standard that state how to calculate this rate.Please note that the client specs did not specify any thing on that. Please send me your thoughts ASAP. ------------------------------------------------------------------------------------------------------------------------------------------------------------------- DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If you have received this communication in error, please notify us immediately by responding to this email and then delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete transmission of the information contained in this communication nor for any delay in its receipt. -------------------------------------------------------------------------------------------------------------------------------------------------------------------
| *** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies." -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment