Sunday, May 9, 2010

Re: [MW:5118] A number for alloy 600(UNS N06600)

Mr. Mahendran,
 
Please refer QW 442. in ASME Sec.IX. A table is provided for 'A' numbers. See the heading ' Classification of Ferrous Weld Metal Analysis for Procedure Qualification' . It gives the weld metal chemical composition of ferrous materials. Since ENiCrFe-3 is a non ferrous consumable (For base metal UNS number coming under ASME Sec.II, Part B) the mentioned A number will not be applicable.
 
If you are looking the A number for WPS/PQR qualification, you can put that column ' N.A'.
 
Regards,
 
Ibrahim PK

On 9 May 2010 12:18, ravishankar menon <ravimenakath@yahoo.co.in> wrote:
Generaly A number  for Filler metal only according to their chmical composition, In your case A number for ERNiCr3 filller wire is 8.


From: mahendran p <pmahe_79@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Sat, 8 May, 2010 10:38:51 AM
Subject: [MW:5107] A number for alloy 600(UNS N06600)

Hi,
    Can anybody tell me what is A - number for the alloy 600(UNS N06600), Filler metal ERNiCr3.
 
Thanks & Regards,
P.Mahendran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate