ERNiCR3 cannot be A No 8. First of all its non ferrous material & Ni% is more is this case (67%min)

On Sun, May 9, 2010 at 12:18 PM, ravishankar menon <ravimenakath@yahoo.co.in> wrote:
Generaly A number  for Filler metal only according to their chmical composition, In your case A number for ERNiCr3 filller wire is 8.


From: mahendran p <pmahe_79@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Sat, 8 May, 2010 10:38:51 AM
Subject: [MW:5107] A number for alloy 600(UNS N06600)

Hi,
    Can anybody tell me what is A - number for the alloy 600(UNS N06600), Filler metal ERNiCr3.
 
Thanks & Regards,
P.Mahendran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...