Hi all,
Refer QW-422 ,if you use A-number 8 will be for Stainless steel .Ther is No A
number for Nickel alloys . You can match the composition in the Table QW-422
vaithiyanathan
On Sun, May 9, 2010 at 12:18 PM, ravishankar menon <ravimenakath@yahoo.co.in> wrote:
Generaly A number for Filler metal only according to their chmical composition, In your case A number for ERNiCr3 filller wire is 8.
From: mahendran p <pmahe_79@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Sat, 8 May, 2010 10:38:51 AM
Subject: [MW:5107] A number for alloy 600(UNS N06600)
Hi,Can anybody tell me what is A - number for the alloy 600(UNS N06600), Filler metal ERNiCr3.Thanks & Regards,P.Mahendran
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
With Best Regards
B.Vaithiyanathan
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment