If feasible you can try Water Jet Cutting !

Regards

Prem Nautiyal

On Thu, 29 Apr 2010 19:42:32 +0530 wrote
>Please check with your machine manufacturer if it is suitable for mixed gas
This will give a far cleaner cut and will remove the possibilities of moisture entering into the plasma stream
Best Regards

PHIL CHEW

Global Segment Manager -Transport ,Shipbuilding,M&R

ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB

Tel: +44 (0) 7584 219132

email: PHIL.CHEW@esab.net

ESAB Holdings Ltd is a company registered in England and Wales . Co registration no 1687590 Registered Office: 322 High Holborn, London , UK , WC1V 7PB www.esab.comPlease consider the environment before printing this email.
From: Pratheesh Chandran [chichuprem@gmail.com]
Sent: 29/04/2010 09:50 ZE4
To: materials-welding@googlegroups.com
Subject: [MW:4994] DSS pipe cutting


dear All
 
Please provide your expertise for the below problem
 
I need to take a branch connection of 4" from a pipe 12" A790 UNS 31803 and had been using plasma cutting to do the same. However soon after carrying out the Plasma cutting it was noticed that the inner wall of 12" pipe starts getting corroded due to the sparks impinching on the inner wall of the pipe  arised during plasma cutting ,( attached Photo graphs )

 Kindly advise  how to avoid  the same  or any other suitable precautionary steps to be taken during cutting  on DSS.
 
Regds
Prem



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...