Re: [MW:4993] API 5L X85 -CVN Requirements

Dear Kathalingam Babu,
                                    
40J (30 Ft-lbf) for pipe in grades > X 80 grade materials & less than 19mm thick. The HAZ for the longitudinal seam weld in HFW welded pipe is usually too narrow to permit accurate sampling for Charpy testing. The requirement for Charpy testing of the seam weld HAZ applies only to SAWL/ SAWH and COWL/ COWH pipe.

 
On Tue, Apr 27, 2010 at 1:22 PM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Gents,
 
Pls tell me, what is the CVN (Longitudinal) Requirements for the API 5L X85 (19 mm thick) ?
 
Thanks & Regards,
 
K.Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Yadav Shiva Chelliya,
Inspection Engineer,
Doha Qatar,
+974-6166465

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...