Hi,
      First of all You have clearly indicate the material spec and product form ,Design code .
 As per ASME B 31.3 you can use upto -425 Deg F(253.8 Deg C)  provided the material is solution annealed condition. Considering the welding the material can be used upto 101Deg F without Impact testing.
 Regards,
 Vaithiyanathan
 On Tue, Apr 27, 2010 at 3:51 PM, KASHKOUSHA <kashkousha1@yahoo.com> wrote:
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
With Best Regards
B.Vaithiyanathan
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments