Hi.
It depend of several variables, if  surface is cleaned, distance between welds, ubication is easy or not, if there are or not many discontinuity, in my experience and for estimation,  I will taken one minute for one inches of weld if there are not many discontinuity and double time if there are.
I hope that the information wiil be help to you.
Best regards.
 
Agustin Jimenez


De: Ali Asghari <asghariali@rocketmail.com>
Para: materials-welding@googlegroups.com
CC: asgharialigl@gmail.com
Enviado: dom, abril 25, 2010 2:39:50 AM
Asunto: [MW:4950] limitation for UT

 
Dear All
is there any limitation length for Ultasonic examination in day?
regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...