Hi,
They may have reservation for not to issue 2.2 test report since 2.2 calls for non specific inspection and testing. non specific means if they check the dimension of the flanges then also it will be not of your lot, such results will not useful to you and secondly this is just jobwork of machining and no testing is involved so that data also they can't provide.

2.2 doesn't call for certification but for only test report.

With Regards,
Rutvik
TATA Projects Ltd.

--- On Fri, 23/4/10, vipin george <vipingeorges@gmail.com> wrote:

From: vipin george <vipingeorges@gmail.com>
Subject: Re: [MW:4940] RE: 4926] 2.2 CERTFICATE
To: materials-welding@googlegroups.com
Date: Friday, 23 April, 2010, 1:57 PM

Hi!
You can ask the supplier to issue a compliance certificate the fitting has been machned from Sch 80 to Sch40

Rgds
Vipin

On Fri, Apr 23, 2010 at 1:07 AM, Elisabeth, Raymond (R) <RELISABETH@dow.com> wrote:
Correct thay are right.
 
Kind regards,

Raymond Elisabeth
Inspection engineer

 
 
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Moen - QA
Sent: Thursday, April 22, 2010 2:15 PM
To: materials-welding@googlegroups.com
Subject: [MW:4926] 2.2 CERTFICATE

Dear member,

We purchase a standard product from manufacturer. The product was '' FLANGE 2 INCH SCH 80 CLS 150 A105'', we received a 3.1 certificate with material, we than ask work shop to machines this flanges to make its ID equal to that of SCH 40 Flanges.

Machining was done in workshop which is ISO 9001-2008 certified. We asked the workshop to issue 2.2 certificates stating that that the product after machining is in conformance with requirement.

However they refused to do so and said that 2.2 certificates can only be issued by a manufacture and since they have not manufactured it they can issue a 2.2 certificate and they will just issue letter.

Is this correct? Can't they issue 2.2 certificates?

Regards


______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...