Re: [MW:4945] FCAW welding for pressure part

incomplete fusion is a major in GMAW with solid wire not with FCAW
kgp

On Wed, Apr 21, 2010 at 11:12 PM, sachin sankhe <sachin.sankhe@rediffmail.com> wrote:
Hi,

We`have FCAW welding for pressure part in refinery service

As FCAW welding mainly have discontinuities like incomplete fusion

So we have specified 100 % RT/MP/DP
However UT is more preferred over RT for planar defect due to incomplete fusion
I feel 100 % RT to be replaced by 100% UT

Request you to give your opinion
Regards
Sachin.Sankhe

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...