Thursday, April 22, 2010

Re: [MW:4922] Re-Certifying Material

hi,
this is very simple.When you recertify ASTM material in to ASME,First you check with the ASME Code book shows Acceptable ASTM edition.According to that you check with ASTM material certificate,whether that edition listed in the ASME or not.If listed than it is ok.Finally you have to check this material properties and Stamp "Material Identical with ASME Edition_________Addenda_________ and Signed by QC Engineer or Manager then it shall be Accepted by AI(If you are doing Code Jobs)If not a Code Jobs Shop QC sign is enough.
 
Regards,
 
(Karthik)

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 4/22/10, Ramesh Barot <rameshnbarot@yahoo.com> wrote:

From: Ramesh Barot <rameshnbarot@yahoo.com>
Subject: [MW:4919] Re-Certifying Material
To: "Materials Welding" <materials-welding@googlegroups.com>
Date: Thursday, April 22, 2010, 4:03 PM

Dear All,
 
Pl.give me detailed procedure for re certifying material?
 
Example 1)ASTM to ASME
              2)AISI to ASME/ASTM
              3)ASME to ASME (Different edition)
 
Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...