The vertical up position typically has the highest heat input which has the greatest effect on impact properties.  Therefore, a PQR qualified in the vertical up will satisfy for the other positions.


Avinash <avinash22285@gmail.com>
Sent by: materials-welding@googlegroups.com

04/20/2010 11:09 AM

Please respond to
materials-welding@googlegroups.com

To
"Materials & Welding" <materials-welding@googlegroups.com>
cc
Subject
[MW:4900] PQR position qualified





Members,

In AWS D1.1, table 4.6 point 6 states that: A 3G vertical up test
qualifies for all positons. If our PQR testing includes CVN
requirement, can we go for only 3G vertical test coupon qualifying all
positons?
Please clarify.

Regards
Avinash

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Subscription settings: http://groups.google.com/group/materials-welding/subscribe?hl=en




----------------------------------------------------------------
This e-mail message and all attachments transmitted with it from the
Nuclear Generation Group of American Electric Power are for the sole
use of the intended recipient(s) and may contain confidential and
privileged information.  Any unauthorized review, use, disclosure or
distribution is prohibited.  If you are not the intended recipient, please
contact the sender by reply e-mail and destroy all copies of the original message.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...