Wednesday, April 21, 2010

Re: [MW:4903] PQR position qualified

Dear Avinash,

Yes, 3G Vertical Up qualifies all positions when CVN required.

If CVN is not required , this variable doesnot apply.

Regards,

K.Babu


----- Original Message -----
From: "Avinash" <avinash22285@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Tuesday, April 20, 2010 11:09 PM
Subject: [MW:4900] PQR position qualified


> Members,
>
> In AWS D1.1, table 4.6 point 6 states that: A 3G vertical up test
> qualifies for all positons. If our PQR testing includes CVN
> requirement, can we go for only 3G vertical test coupon qualifying all
> positons?
> Please clarify.
>
> Regards
> Avinash
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> Subscription settings:
> http://groups.google.com/group/materials-welding/subscribe?hl=en
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...