Re: [MW:4902] repair of toe crak

how much does exceed the accumulated length of crack, that the whole length of the weld shall be gouged and cut out?
in which refrence document, it is mentioned(preferably in structural fabrication)?

On Tue, Apr 20, 2010 at 11:57 AM, <george.dilintas@gr.bureauveritas.com> wrote:

UT is the best solution. Detection will be done from the flange surface of the T joint.
You may start with longitudinal waves and then recheck with transversal waves


Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for ali asghari <asgharialigl@gmail.com>ali asghari <asgharialigl@gmail.com>



To

materials-welding@googlegroups.com

cc


Subject

[MW:4892] repair of toe crak

Ref


Dear All
in my project, after plate girder fabrication( with thickness of 35 to 50) in Tjoint that have double bevel joint, longitudinal crack in parent metal( that discontinuted) detected by MT in 6M length.
with grinding of a small part , it finded that the depth of crack is approximately 7mm.
now how can i remove this doubt that may be there are branches of crack in lower depth or close the root of double bevel?( how can i trust to UT to detectability?)
does anyone have procedure or recommendation about removing and repair of them?
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...