Re: [MW:4685] NDT requirements for API 650 Tanks

My friend.
 
Tee joints should be Radiograph @ 100%, remaining @ 10%

 

Regards

 

Syed Arshad Farooq 

 QA / QC Engineer

 PROCTER & GAMBLE

 D.L UNIT KARACHI

(+92-21-111-284-284,5378637-40

): +92-308-3067599




From: Subramani <subramak@batelco.com.bh>
To: materials-welding@googlegroups.com
Sent: Sun, April 4, 2010 9:14:01 AM
Subject: [MW:4681] NDT requirements for API 650 Tanks

Hi,
Can anybody clarify the percentage NDT requirements: type of NDT, coverage etc, for tanks made to API 650.  
 
Regards,
Subramani.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...