dear All
 
Please provide your expertise for the below problem
 
I need to take a branch connection of 4" from a pipe 12" A790 UNS 31803 and had been using plasma cutting to do the same. However soon after carrying out the Plasma cutting it was noticed that the inner wall of 12" pipe starts getting corroded due to the sparks impinching on the inner wall of the pipe  arised during plasma cutting ,( attached Photo graphs )
 Kindly advise  how to avoid  the same  or any other suitable precautionary steps to be taken during cutting  on DSS.
 
Regds
Prem

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...