[MW:4943] SS410S material -Pickling & passivation

Dear All,
 
I am working as a static equipment engineer for refinery&petrochemical projects.
 
As per Owner requirements All SS tray assemblies to be pickled & passivated.
 
Howeever the tray vendor claims it is not applicable for SS410S as pickling & passivation may lead to white & brown pathches on trays.
 
Please clarify if pickling & passivation for SS410S (martensitic grade) materials is applicable or not?
 
Awaiting your prompt response.
 
 
Yours
 
Salman Hussain,Baroda,India.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...