Sunil,
A ferrite content range of 2 to 8% is equivalent to a ferrite number range of 2 to 8.5. You can check the Delong-WRC diagram to double check.
Regards,
Seth Norton
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Agrawal Sunil (Mumbai -Stequ)
Sent: Wednesday, March 31, 2010 10:05 PM
To: 'materials-welding@googlegroups.com'
Subject: [MW:4652] Ferrite Number Vs Ferrite Content
Can anyone guide me what is the difference between Ferrite Number and Ferrite Content?
Our client has asked for ferrite content to be limited within 2 to 8% is SS. Whereas our Licensor (KBR) practice is to specify the FN (ferrite number). What value (FN) our Licensor should specify in their process datasheet which is equivalent to 2 to 8% ferrite content?
Please guide me.
Best Regards,
Sunil Agrawal
Tecnimont ICB
Comments
Regards,
Ashfaq Anwer
http://forums.thepetrostreet.com