[MW:3349] Re: Hydrotest flange thickness calculation


Chaitanya ,

Find out whether this is cross country pipeline or belongs to any petrochemical plant , because code limitation will differ , ASME B 31.3 has calculations about Blind flange , but size may limited


Thanks & Best Regards,

Vinayak Kale
E & C  DIv. QA & I , OGSP
Larsen And Toubro Ltd
Powai , Mumbai
vinayak_kale@lntenc.com
Ph No.+91- 67053805/3685
Fax No. +91-67051988
(M) - + 91 9892743803



Chaitanya Purohit <chaitanya_purohit@yahoo.co.in>
Sent by: materials-welding@googlegroups.com

09/27/2009 07:06 PM

Please respond to
materials-welding@googlegroups.com

To
Material Welding <materials-welding@googlegroups.com>
cc
Mithun.Murali@dodsaldxb.ae
Subject
[MW:3336] Hydrotest flange thickness calculation





Dear Friends,

Please help to reply to the below query....

---------- Forwarded message ----------
From: Mithun Murali <
Mithun.Murali@dodsaldxb.ae>
Date: 2009/9/27
Subject: Query regarding Hydrotest flanges
To:
chaitanya_purohit@yahoo.co.in

Hi Chaitanya,

Can you ask this query in the group as I am unable to do so.

Any calculation sheet or method available for Thickness calculation for Blind Flange for 64 " CS pipeline hydrotest.(test pr of 83 barg), 400# rating.

I had referred to one of the Client spec, which demands 170mm thick plates for the same.

Any reference of Agency or Consultant doing these kind of Calculations.

 

Thanks and regards,

Mithun

Design Engineer - Piping

Dodsal Engineering & Construction Pte. Ltd.

Dubai, U.A.E.

Phone : +9714-3161279




Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...