[MW:3340] Re: ACCEPTANCE OF ROUNDED INDICATION BY VISUALL INSPECTION

Dear Mr. Azmi
 
A pin hole of 5mm deep in a weld of only 6mm detected by visual examination is not accceptable. 
Gopu

--- On Mon, 28/9/09, asad azmi <azmiasadayub@gmail.com> wrote:

From: asad azmi <azmiasadayub@gmail.com>
Subject: [MW:3338] ACCEPTANCE OF ROUNDED INDICATION BY VISUALL INSPECTION
To: materials-welding@googlegroups.com
Date: Monday, 28 September, 2009, 1:05 PM

GOODMORNING...........
 
can anybody can confirm  whether a pin hole of diameter 3mm and depth of approximately 5 mm in fillet weld  of 6mm of material SA 516GR 70  can be VISUALLY accepted. The vessel is fabricated as per ASME SEC VIII DIV 1.
 
If YES then by which code.
 
Kindly note that if we consider acceptance crieteria  for PT/MT, as per ASME SEC VIII DIV 1, APPENDIX 6/8, Rounded indication upto 4.8mm is acceptable.
 
can the above defect can be accepted on the basis of acceptance crieteria of PT/MT.
 
 
please reply ASAP.
 
Thanks & Regards
 
Asad Azmi


On Thu, Sep 24, 2009 at 1:35 PM, Adi <adinraos@gmail.com> wrote:


If joint repair came in 2" pipe, it is very difficult to identify
repair the exact location & root repair we can't do, so the joint
should be cut out
My question is When we are calculating the welders repair %  we have
to consider total length of 2" is repair ? Why because we repaired the
total length
Is it correct please advice

Adi


Connect more, do more and share more with Yahoo! India Mail. Learn more
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...