Skip to main content

[MW:3270] Re: [MW:/] Re: 3238] Shelf life of Low hydrogen electrodes

Dear Friend
 
The shelf life of electrodes is directly depended on the storage condition which are not clearly known for you. As you know basic electrodes types are so sensitive to humidity absorption. Accordingly it is recommended to visually random check of some baches and inspecting the tencity of the rod covers by bending them and also soundness of rod.( Having no corrosion)
Furthermore you could test a random batch of these electrodes by changing the welding parameters in work shop before commence of project.
Anyway consulting with manufacturer would be also useful.
 
Yours truly,
K.Alyari

 
On 9/22/09, rajagopal kannan <rajagopal.kannan@gmail.com> wrote:
Dear Shasank,
As stated in this tread earlier, ASME Sec. IX code does not state anything about this. we have to go by tthe manufacturer's instruction only.
But, I have come across a practice to test its usability. But I can't provide you any type of written reference. It was found in one of the vendor's system procedures.

Electrodes considered as old, which doesn't loose flux when dropped vertically from 1 meter height from ground is suitable for welding.

You can try this.
Thanks and Best Regards,
K.Rajagopal


 
On Fri, Sep 18, 2009 at 7:16 AM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Hi,
All Ok and accordingly noted. How about the shelf life, if the packing is not damaged, do we follow manufacturer's instructions or is there any expiry date for it? What is the general approach here, in absence of anything else?
Regards,
Shashank Vagal

--- On Thu, 17/9/09, claes.gillenius@esab.se <claes.gillenius@esab.se> wrote:

From: claes.gillenius@esab.se <claes.gillenius@esab.se>
Subject: [MW:3240] Re: 3238] Shelf life of Low hydrogen electrodes Date: Thursday, 17 September, 2009, 4:11 PM



If the electrodes are packed in air tight packages they can be used right away. If not, redry the electrodes in the way the manufacturer recommends, normally at a temperature around 300 - 350 °C.
Air tight packages are for example vacuum packages. If such a package is damaged and the vacuum lost, redy the electrodes. Redrying returns the electrodes to it´s original state.

Best regards,

Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                                 Lindholmsallén 9
Company  reg number        556005-7738



"Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com>
Sent by: materials-welding@googlegroups.com

2009-09-17 12:17


To
<materials-welding@googlegroups.com>
cc

Subject
[MW:3239] RE: 3238] Shelf life of Low hydrogen electrodes







Consult the consumable manufacturer, may be shelf life revalidated with additional testing. Code does not specify the shelf life, but the manufacturer does.



From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ravindra T
Sent:
Thursday, September 17, 2009 3:28 PM
To:
materials-welding@googlegroups.com
Subject:
[MW:3238] Shelf life of Low hydrogen electrodes

 
Dear All
 
Our contractor has brought low hydrogen electrodes (E 7018 & 8018) which are manufactured in 2007 for welding station piping in one of our intermediate pump station of our cross country pipeline project. I would like to know whether these electrodes can be used now?. Is there any reference in ASME code regarding the expiry/ shelf life of Electrodes?
 
Please advise me in this regard.
 
Thanking you all in advance
 
Ravindra
Senior Project Engineer






This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

 



From cricket scores to your friends. Try the
Yahoo! India Homepage!

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...