Skip to main content

[MW:3309] Re: application of SS Flux cored wire for GTAW, SFA 5.22

Yes, STT is a good option only if you could use GMAW process. And its worth an investment only if such jobs are regular.

Besides STT, even Miller Electric has developed their patented technology RMD - Regulated Metal Deposition. Machine Model is Pipepro 450. Its somewhat similar to STT and a little more to offer. check www.millerwelds.com

Regards

VISHAL



On Fri, Sep 25, 2009 at 8:54 AM, vipin george <vipingeorges@gmail.com> wrote:
Dear Bathula,
 
A new process is developed by Lincoln STT(Surface tension transfer) it's GMAW process with short circuit transfer.It's good for piping applications.Check Lincol electric.

Regards,
vipin


On Tue, Sep 22, 2009 at 12:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Dear members

We have typical vessel (site assembly), where backing gas arrangement could not be done for a stainless steel joint due to Safety (confined space), as well as space constraint.

One of the options will be using flux cored wire for GTAW.

Please share your view on these consumables for root pass of GTAW Stainless steel; where backing gas application is impractical, any body used these consumables?

Kobleco is manufacturing these wires under TGX series, any other manufactures who has similar product for this application?










--
SUPERTECH SERVICES LTD
Plot A-253, Road 30B,
Wagle Indl Estate,
Thane W 400 604
Maharashtra, India
Tel: +91-22-25826190/91
Fax: +91-22-25826189
Email: vdm@supertechservices.in
Web: www.supertechservices.in

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...