Thank Q to all

 

If I calculate full cut out (especially for 2") The repair % is coming too much

Exp: 10 joints 1 joints repair means 10%repair rate

However the repair portion is very small, I have to cut the joint

 

Observed welder repair rate above 5%, he should be taken off the job and sent for re-training for a week.. ok

After requalification his repair % calculation start from fresh or from the old ?

 

Adi


 
On 9/25/09, Shashank Vagal <nach_sam@yahoo.com> wrote:
Hi,
Whatever amount of repair was caused by the welder and no. of joints repaired should be attributed fully to him. Indication type etc are immaterial, it is the bad workmanship that we are considering. And indication is repairable if it is a defect (not acceptable), right? Indicates bad workmanship. Accordingly it needs to be treated. But a record can be kept of % length repaired, just for comparison. Otherwise, it is for the % repair rate per joint that a welder's record should be maintained. Just for your info, If the repair rate shows sign of exceeding 1.5%, the welding supervisor should take cognizance. If it is >3%, the welder should be warned officially. Above 5%, he should be taken off the job and sent for re-training for a week. These are the general norms in the welding world in the industry. Or, so my notes say.
Shashank Vagal

--- On Thu, 24/9/09, MNS <mn.senthilkumar@ymail.com> wrote:

From: MNS <mn.senthilkumar@ymail.com>
Subject: [MW:3303] Re: Welder reapir %
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Thursday, 24 September, 2009, 5:49 PM


If it is cut and reweld, 100% repair to be considered for quality
costing; but, for welder performance, the actual repair/defect % only
to be considered - this is just a thought....

Thanks
Senthil

On Sep 24, 3:35 pm, Adi <adinr...@gmail.com> wrote:
> If joint repair came in 2" pipe, it is very difficult to identify
> repair the exact location & root repair we can't do, so the joint
> should be cut out
> My question is When we are calculating the welders repair %  we have
> to consider total length of 2" is repair ? Why because we repaired the
> total length
> Is it correct please advice
>
> Adi


Yahoo! India has a new look. Take a sneak peek
SEPOC
TC-8112
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...