[MW:3007] RE: 3005] Re: ASME Sec-IX ( QW-403.5) interpretation

Yes, you can use it in the 3 situations but you can't change any of the qualified variables of the PQR.
And it is not probably that you use E 309MoL to joint P1-P1, isn´t it?


 
 
02965 451-342 (6413) /// 02965 15267865

-----Mensaje original-----
De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de MNS
Enviado el: lunes, 24 de agosto de 2009 8:02
Para: Materials & Welding
Asunto: [MW:3005] Re: ASME Sec-IX ( QW-403.5) interpretation


(i) **P-No. 1 Gr.No.2 to P-No. 1 Gr.No.2 - Answer
is NO

(ii) **P-No. 1 Gr.No.2 to P-No. 8 Gr.No.1 - Answer
is YES

(iii) **P-No. 8 Gr.No.1 to P-No. 8 Gr.No.1 - Answer is
No

Thanks
Senthil


On Aug 24, 8:57 am, Kural <kura...@gmail.com> wrote:
> Interpretation: Answer is yes ( for all 3 combination of basemetals) as long
> as other essential and supplemtary essential are unchanged.
>
> On Sun, Aug 23, 2009 at 9:48 PM, Sukamal Naskar <sukamalbec...@gmail.com>wrote:
>
>
>
> > Dear All,
> > Good Morning !!!
>
> > I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )
>
> > QW-403.5 (c ) , states that " --------------- In addition, when base
> > metals of two different P-Number Group Number combinations are qualified
> > using a single test coupon, that coupon qualifies the welding of those two
> > P-Number Group Numbers to themselves as well as to each other using the
> > variables qualified."
>
> > *Query: If we qualify one PQR, with P-No. 1 Gr. No 2 to P-No.8 Gr.No.1
> > material using SMAW ( E 309MoL) process with impact testing on weld metal
> > & both HAZ portion , does this PQR supports the following WPS combination of
> > base metals , if all other welding variables are unchanged ?*
>
> > * *
>
> > *(i) **P-No. 1 Gr.No.2 to P-No. 1 Gr.No.2 *
>
> > *(ii) **P-No. 1 Gr.No.2 to P-No. 8 Gr.No.1 *
>
> > *(iii) **P-No. 8 Gr.No.1 to P-No. 8 Gr.No.1 *
>
> > Please give your comments,
>
> > Thanking you,
> > Regards,
> > --
> > Sukamal Naskar
> > Malaysia- Hide quoted text -
>
> - Show quoted text -


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...