Skip to main content

[MW:3059] Re: Formula for calculating SMAW & TIG Consumable Quantity & Gas Consumption

Friends ,
 
thanks for hte below guide line ,
 
Here i am looking for more details instead of knowing the whole volume of metal required .
 
I would lke to know the quantity for each type of electrode as we have for eg TIG root and hot pass followed with 7016 or
 
root is down hill and the other pasess are up hill ,
 
Do any one know how to find this or any Excel  program as most of the time need to depend of the supplier or welding formans .
 
Any helping hand will be appreciated .
 
Regards
 
Sujeet
On Wed, Aug 26, 2009 at 4:30 PM, daniel iordache <daniel.iordache@gmail.com> wrote:
Hi,

maybe that help you ....

in part ....

Regards

On Wed, Aug 26, 2009 at 8:12 AM,
chandergirotra@gmail.com<chandergirotra@gmail.com> wrote:
>
> REPLY
>
> Dear Member/s,
>
> THe quickest method is to fist  calculate volume of  the V- groove .
> Multiply this volume with density to get theoreticall weight of weld
> metal. Now we know that the actual weight used is much more than the
> theoretical weight since there are butt losses,electrode coating has
> to be accounted for and there is convexity at the top and  root of
> joint.
> Thus the  weld metal weight therefore =theoretical weight xQ factor
> ( Quantity  factor) .This Q factor=2 for TIG welding and 2.5 for SMAW.
>
> Hope this thumb rule will help you calculate weight of  welding
> electrode/wire required for a joint..
>
> Sorry that for your second query for gas consumption I am unable to
> respond.
>
> Chander Girotra
> ==========================================================================================================================
>
> On Aug 25, 2:48 pm, Sujeet Sangle <sujeetsan...@gmail.com> wrote:
>> Dear Memebers ,
>>
>> I need to calculate quantity for SMAW consumable  for Structural Electrodes
>> for V Groove different thickness and Diameter
>>
>> TIG consumable for piping work different thickness and Diameter .
>>
>> Together with the Pre heating gas consumption .
>>
>> Can any one guide me for the above .
>>
>> Thanks
>>
>> Sujeet
>
> >
>



--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...