Interpretation:

1X-89-75

IX-89-75,M -89-76

Subject: Section

Ix, QW-403.5, .QW-403.11, and QW-424

Date Issued: September 20, 1990

File: BC90-443

Question (1):

A procedure qualification using the SMAW process in a V-groove joint has been

qualified with acceptable bends, tensiles and charpy V-notch impact specimens, using P-No.

1 Gr.

No.

2 material welded to a P-No. 3 Gr. No. 3 material. Does the procedure qualification support

the welding

of P-No. 1 Gr. No. 2 material together when notch toughness tests are required?

Reply (1): No.

Question

(2): Does the procedure qualification support the welding of P-No. 1 Gr. No. 2

material to P-No.

3 Gr. No. 3 material?

Reply

(2): Yes.

Question

(5): Does the procedure qualification support the welding of P-No. 3 Gr. No. 3

material together?

Reply

(3): No.

 


On Sun, Aug 23, 2009 at 10:10 PM, Sayee Raghunathan <Sayee.Raghunathan@twi.co.uk> wrote:

No, QW-403.5 applies for Group number combinations not P-Number. Always remember in Section IX to go as per tables in QW250 and associated tables. SO for eg., QW-253 for SMAW states for Group Nos, Ø Group No as per QW-403.5 and Ø P-No as per QW 403.11 are supplementary essential and essential variables respectively. This implies that for your enquiry below, separate PQRs are required for each material combination specified.

--------------------------------------------
USE OF INFORMATION - The advice given by TWI has been given in good faith and on an impartial basis, being based solely on the information received from the Client.  The Client shall not, without the written permission of TWI, use or reproduce the information in full or in part in any advertising copy, sales or promotion literature, or for any other publicity purpose nor use any information from TWI as evidence in disputes, litigation or other legal action.
--------------------------------------------
Thanks and Regards
Sayee P Raghunathan
Cert.EWE CEng SenMWeldI MIMMM
Duty Engineer
TWI Ltd.
Granta Park
Great Abington
Cambridge CB21 6AL
United Kingdom
EMail: duty.engineer@twi.co.uk
Web:   http://www.twi.co.uk <http://www.twi.co.uk/>
Tel:  +44(0)1223 899000
Fax: +44 (0) 1223 892588

Seeking Technical Information? Industrial Members can access data as JoinIT registrants at http://www.twi.co.uk <http://www.twi.co.uk/>
When sending e-mails to TWI please help us by including your personal name, company name, and contact details in your e-mail signature, in a format similar to that used above. Please note that the information given above represents experience and opinion and does not reflect any code or standard and is intended for the recipient only.




________________________________

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kural
Sent: 24 August 2009 04:58
To: materials-welding@googlegroups.com
Subject: [MW:2998] ASME Sec-IX ( QW-403.5) interpretation


Interpretation: Answer is yes ( for all 3 combination of basemetals) as long as other essential and supplemtary essential are unchanged.




On Sun, Aug 23, 2009 at 9:48 PM, Sukamal Naskar <sukamalbecmet@gmail.com> wrote:


       Dear All,
       Good Morning !!!

       I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )


       QW-403.5 (c ) , states that " ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."



       Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1 material using  SMAW ( E 309MoL) process with impact testing  on weld metal & both HAZ portion , does this PQR supports the following WPS combination of base metals , if all other welding variables are unchanged ?



       (i)                  P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2

       (ii)                P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1

       (iii)               P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1



       Please give your comments,



       Thanking you,

       Regards,
       --
       Sukamal Naskar
       Malaysia











TWI Ltd
Registered Number: 3859442 England
Registered Office: Granta Park, Great Abington, Cambridge, CB21 6AL, UK

_______________________________________________________________________
The information in this e-mail is confidential, and may be legally
privileged.  It is intended only for the person(s) specified in the
above address.  Access to this e-mail by anyone else is unauthorised,
and any disclosure, copying, distribution or other use of this e-mail
is prohibited and may be unlawful.  We will not under any circumstances
have any responsibility or liability arising out of or in connection
with any unauthorised use of this e-mail.  Please inform us if this
message has gone astray before deleting it.

Please note that all e-mail is monitored.

When sending e-mails to TWI, please help us by including your name,
company, and details in your e-mail signature.

Seeking Technical Information? Industrial Members can access data as
JoinIT registrants on http://www.twi.co.uk
_______________________________________________________________________






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...