[MW:2999] Re: 2996] Technical Query on ASME Sec-IX ( QW-403.5)

Dear Mr. Bathula Raghuram ,
 
Thanks for your response,
Can you please explain what does it mean by 
 " ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."
It seams that it can be two different P numbers also.
 
Please give your views...
 
thanking you,
 
Regards
 


On Mon, Aug 24, 2009 at 11:59 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

No,

It applies to different group number within same P number, and not with different P numbers.

Any way why you are impact testing this combination (P1 # P8), what are your design conditions?

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sukamal Naskar
Sent: Monday, August 24, 2009 9:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:2996] Technical Query on ASME Sec-IX ( QW-403.5)

 

Dear All,

Good Morning !!!

 

I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )

 

QW-403.5 (c ) , states that " ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."

 

Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1 material using  SMAW ( E 309MoL) process with impact testing  on weld metal & both HAZ portion , does this PQR supports the following WPS combination of base metals , if all other welding variables are unchanged ?

 

(i)                  P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2 

(ii)                P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1 

(iii)               P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1 

 

Please give your comments,

 

Thanking you,

Regards,
--
Sukamal Naskar
Malaysia







--
Sukamal Naskar
Malaysia



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...