thanks Mr. Srinivas

sorry i have to issued again my questions......

1. so...i have 2 x 10" pipeline ....under API 1104 10 % RT inspection
outside of plant .....

What happen with the part of pipeline inside de plant ...will be also
10% according Api 1104 or will be under B31.3 with 5% RT
inspection....iI mention that the pipelines contain one bitumen and
second one gasoil ....

2. Along the bitumen pipeline and piping system i have a 1" hot oil
traced pipe .....that mantain the main line hot

What kind the inspection should be apply for above pipe and what percentage ....

Thank you on advance.....

Daniel

On Thu, Aug 20, 2009 at 2:20 PM, sreeram64 .<sreeram64@sify.com> wrote:
> Dear Daniel
>
> The clear answer to your query is inspection as per API1104.   For the
> pipeline you mentioned falls as per ANSI B 31.8....
>
> With regards,
> Sreeram_Srinivas
>
> On Thu, Aug 20, 2009 at 3:48 PM, daniel iordache <daniel.iordache@gmail.com>
> wrote:
>>
>> Dear all,
>>
>> We have to build two 10" pipelines according Api 1104- one bitumen in
>> concrete trench and other by gas oil (buried)... we have 10% RT
>> .....but a part of lines are inside plant (around 30 meters -15
>> welds.....)
>> how we will inspect RT the welds inside plant ...according API or B31.3?
>>
>> Also along the bitumen piping system and pipeline we have 1" hot oil
>> traced line .....
>> What kind of inspection is recommended? RT%? PT%? Visual?
>>
>>
>> Thanks
>>
>> Daniel
>>
>> >>
>
>
>
> --
>
>
> With regards,
> Sreeram_Srinivas
>

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro: +40721731728
E-Mail: daniel.iordache@gmail.com
daniel_iordache@yahoo.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...