[MW:3093] Re: Coating material for LTCS bolts on SS 304 flanges

Dear Agustin,
 
thanks a lot for your slon.
 
do you have any procedure for this....
Please send me the information.if u have...
 
Your reply appreciated in advance..
 
Regards,
 
Prakash K B

 
On 8/31/09, AGUSTIN JIMENEZ <agumarca@yahoo.com> wrote:
Too try use insulating gasket for bolts and nuts.
excuse me if my english is not good.
 
Regards
Agustin Jimenez 
 


De: Nilesh Pathare <patharenil@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: lunes, 31 de agosto, 2009 5:15:46
Asunto: [MW:3088] Re: Coating material for LTCS bolts on SS 304 flanges

You can go for FBE ( Fusion Bonded Epoxy) coating for those bolts.
FBE coating is a good option. But check other parameters and the fluid if its affect the FBE material.

Regards,
Nilesh Pathare.


On Fri, Aug 28, 2009 at 2:48 PM, prakash kamathuru <prakashkbp@gmail.com> wrote:
Dear all,
 
Can any one help me to find the coating material for A320 Gr L7 bolts and A 194 Gr 2 nuts on SS 304 Flanges.As i checked the galvonic series Zn/mg not recomnded.Presently this heat exchnger flange which is already installed at site.Any Solution,so that without disturbing the joint we can coat some material at site for controlling galvonic corrosion.
 
Please keep in mind that it is STHE body flange.
 
Your feedbacks very helpful for me in taking decision and appriciated.
 
Regards,
 
Prakash





--
Best Regards,

Nilesh Pathare
 



¡Obtén la mejor experiencia en la web!
Descarga gratis el nuevo Internet Explorer 8
http://downloads.yahoo.com/ieak8/?l=e1


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...