Tuesday, March 5, 2019

Re: [MW:29197] REQUALIFICATION OF PQR

Dear Venkat.
Based on which paragraph.
Regards.

On Tue, Mar 5, 2019 at 11:24 AM 'venkat chikkala' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear all,

If all essential veriables are unchanged, impact test is enough.

Regards,
CH V RAMANA

On Tuesday, 5 March, 2019, 12:23:23 pm IST, <asgharialigl@gmail.com> wrote:


Dear All.

If a supplementary essential variable changed such as group no., now the new PQR just need to be impact tested or other mechanical tests also needed to repeat?

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/LgD4vVMvN5c/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...