Hello,
You may make a new test coupon with the same welding parameter. Then send to restest and update to PQR.
Bien ND
Sent from my Blackberry
From: 'venkat chikkala' via Materials & Welding Sent: Tuesday, March 5, 2019 14:54 To: materials-welding@googlegroups.com Reply To: materials-welding@googlegroups.com Subject: Re: [MW:29194] REQUALIFICATION OF PQR |
Dear all,
If all essential veriables are unchanged, impact test is enough.
Regards,
CH V RAMANA
On Tuesday, 5 March, 2019, 12:23:23 pm IST, <asgharialigl@gmail.com> wrote:
Dear All.
If a supplementary essential variable changed such as group no., now the new PQR just need to be impact tested or other mechanical tests also needed to repeat?
Regards.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment