Skip to main content

Re: [MW:28936] IF ans IFD as per API 1104

AUT is mandatory by Client spec.


And Client spec not accepting Lack of fusion. 

We are getting Lack of Fusion and LFD on almost every joint.  Intention of post is to seeking justification for accepting LFD. Client telling as per API 1104 both IF and IFD are Lack of Fusion only hence needed to be CUT OUT and Rewelded. 

I am seeking advice from experts here to justify client regarding the acceptance of LFD 



With Regards
Riaz 
 

On Thursday, 17 January 2019 09:23:56 UTC+5:30, Muneeb wrote:
Hi,

Who told you to perform AUT? I mean why not RT? AUT will hold your project in Reverse gear.

Mostly in stringent case we perform AUT/PAUT/TOFD or where there is multiple requirement like tie-in's, anyhow it's mutual agreement between company and contractor.

And yes both are different by 9.3.4 / 9.3.5, ID and IFD, you cannot straight away reject but contemplate upon given para condition as per the pipe sizes then proceed for acceptance/rejections.

Thanks
Muneeb

On Wed, Jan 16, 2019, 9:24 PM Ri@z <riaz.r...@gmail.com> wrote:

Dear All,

Our Pipeline specification not accepting Incomplete Fusion .In case of incomplete fusion weld shall be rejected and re-welded.


But according to API 1104, IF and IFD are different . So is it required to reject both IF and IFD as both are incomplete Fusion?

Please help me with advice 


I am using AUT for the inspection and 70 % of joints are detecting either IF or IFD 




With Regards

Riaz 





Pls help me 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...